Composition
2 micrographs for composition Cu 70, Zn 30 (wt%) (pure), ordered by micrograph number.
![]() |
Micrograph
425
:
Cu 70, Zn 30 (wt%) (pure) brass, dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) (pure) Reflected light microscopy 800 μm |
![]() |
Micrograph
426
:
Cu 70, Zn 30 (wt%) (pure) brass, dendritic solidification System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) (pure) Reflected light microscopy 400 μm |