Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Composition
2 micrographs for composition Cu 65, Zn 35 (wt%) (pure), ordered by micrograph number.
![]() |
Micrograph
447
:
Cu 65, Zn 35 (wt%) B4 brass, chill cast System: Cu-Zn, Composition: Cu 65, Zn 35 (wt%) (pure) Reflected light microscopy 400 μm |
![]() |
Micrograph
448
:
Cu 65, Zn 35 (wt%) B4 brass, chill cast System: Cu-Zn, Composition: Cu 65, Zn 35 (wt%) (pure) Reflected light microscopy 200 μm |