Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Composition
7 micrographs for composition Cu 50, Zn 50 (wt%), ordered by micrograph number.
![]() |
Micrograph
458
:
Brass, exhibiting grain boundary nucleation System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
459
:
Brass, exhibiting grain boundary nucleation System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
460
:
Brass, exhibiting grain boundary nucleation System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
468
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
469
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
470
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
471
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |