Composition
6 micrographs for composition Cu 90, Sn 10 (wt%), ordered by micrograph number.
![]() |
Micrograph
494
:
Cu 90, Sn 10 (wt%) bronze, as cast System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
495
:
Cu 90, Sn 10 (wt%) bronze, as cast System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
496
:
Cu 90, Sn 10 (wt%) bronze, as cast System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
497
:
Cu 90, Sn 10 (wt%) bronze, cast annealed System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
498
:
Cu 90, Sn 10 (wt%) bronze, cast annealed System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
499
:
Cu 90, Sn 10 (wt%) bronze, cast annealed System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) Reflected light microscopy 100 μm |