Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Composition
3 micrographs for composition Cu 98, Be 2 (wt%), ordered by micrograph number.
![]() |
Micrograph
38
:
Cu 98, Be 2 (wt%), slow cooling - annealing twins System: Cu-Be, Composition: Cu 98, Be 2 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
39
:
Cu 98, Be 2 (wt%), quenched and aged - annealing twins System: Cu-Be, Composition: Cu 98, Be 2 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
40
:
Cu 98, Be 2 (wt%), quenched and aged - annealing twins System: Cu-Be, Composition: Cu 98, Be 2 (wt%) Reflected light microscopy 80 μm |