Composition
4 micrographs for composition Cu 88, Sn 8, Zn 4 (wt% approx), ordered by micrograph number.
![]() |
Micrograph
516
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 800 μm |
![]() |
Micrograph
517
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 400 μm |
![]() |
Micrograph
518
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 200 μm |
![]() |
Micrograph
519
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 100 μm |