Composition
3 micrographs for composition Cu 95, Sn 5, P 0.15 (wt% approx), ordered by micrograph number.
![]() |
Micrograph
520
:
Cu - 5% Sn phosphor bronze. System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx) Reflected light microscopy 400 μm |
![]() |
Micrograph
521
:
Cu - 5% Sn phosphor bronze. System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx) Reflected light microscopy 200 μm |
![]() |
Micrograph
522
:
Cu - 5% Sn phosphor bronze. System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx) Reflected light microscopy 100 μm |