Composition
3 micrographs for composition Cu 90, Sn 10 (wt%) + P trace, ordered by micrograph number.
![]() |
Micrograph
523
:
Phosphor bronze exhibiting cored dendrites. System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) + P trace Reflected light microscopy 400 μm |
![]() |
Micrograph
524
:
Phosphor bronze exhibiting cored dendrites. System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) + P trace Reflected light microscopy 200 μm |
![]() |
Micrograph
525
:
Phosphor bronze exhibiting cored dendrites. System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) + P trace Reflected light microscopy 100 μm |