Composition
108 micrographs for composition Not specified (System: Zn), ordered by micrograph number.
Showing 1 - 10 of 108 micrographs | Page 1 2 3 4 5 6 7 .. 11 | Previous | Next |
![]() |
Micrograph
41
:
Zn, cold rolled - mechanical twins System: Zn, Composition: Not specified Reflected light microscopy 400 μm |
![]() |
Micrograph
42
:
Zn, cold rolled - mechanical twins System: Zn, Composition: Not specified Reflected light microscopy 80 μm |
![]() |
Micrograph
144
:
Zinc, notched specimen, failed through brittle cleavage fracture. System: Zn, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
145
:
Zinc, notched specimen, failed through brittle cleavage fracture. System: Zn, Composition: Not specified Scanning electron microscopy (SEM) 1 mm |
![]() |
Micrograph
872
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production. System: Zn, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
873
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production. System: Zn, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
874
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production. System: Zn, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
875
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production.. System: Zn, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
876
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production. System: Zn, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
877
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production. System: Zn, Composition: Not specified Reflected light microscopy 500 μm |