Composition
1 micrograph for composition Araldite CT200/HT907 'matrix' with ellipsoid CT200/HT901 'particle', ordered by micrograph number.
![]() |
Micrograph
599
:
Frozen stress photoelastic assessment of load distribution around an ellipsoid System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with ellipsoid CT200/HT901 'particle' Cross-polarised light microscopy 6 mm |