Composition
1 micrograph for composition Al, Mg 2.5 (wt%), with Al2O3 (5 vol%), ordered by micrograph number.
![]() |
Micrograph
603
:
Section of a metal matrix composite (MMC) System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (5 vol%) Reflected light microscopy, polarised 80 μm |