Composition
5 micrographs for composition Al 10, Cu 90 (wt%), ordered by micrograph number.
![]() |
Micrograph
665
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
666
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
667
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
668
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
669
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 20 μm |