4 micrographs for composition Magnesia 85, chromite 15 (wt%), ordered by micrograph number.
![]() |
Micrograph
675
:
Magnesia-Chromite Clinker System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
676
:
Magnesia-Chromite Clinker System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
677
:
Magnesia-Chromite Clinker System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
678
:
Magnesia-Chromite Clinker System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%) Reflected light microscopy 50 μm |