4 micrographs for composition Not specified (System: BaO-Nd2O3-4TiO2), ordered by micrograph number.
![]() |
Micrograph
679
:
BaO-Nd2O3-4TiO2 System: BaO-Nd2O3-4TiO2, Composition: Not specified Reflected light microscopy 400 μm |
![]() |
Micrograph
680
:
BaO-Nd2O3-4TiO2 System: BaO-Nd2O3-4TiO2, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
681
:
BaO-Nd2O3-4TiO2 System: BaO-Nd2O3-4TiO2, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
682
:
BaO-Nd2O3-4TiO2 System: BaO-Nd2O3-4TiO2, Composition: Not specified Reflected light microscopy 50 μm |