5 micrographs for composition Not specified (System: Cu-P), ordered by micrograph number.
![]() |
Micrograph
705
:
Cu-? wt% P System: Cu-P, Composition: Not specified Reflected light microscopy 400 μm |
![]() |
Micrograph
706
:
Cu-? wt% P System: Cu-P, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
707
:
Cu-? wt% P System: Cu-P, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
708
:
Cu-? wt% P System: Cu-P, Composition: Not specified Reflected light microscopy 50 μm |
![]() |
Micrograph
709
:
Cu-? wt% P System: Cu-P, Composition: Not specified Reflected light microscopy 20 μm |