Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Composition
3 micrographs for composition Fe, C 3.2, Si 2.5, Mg 0.05 (wt%), ordered by micrograph number.
![]() |
Micrograph
779
:
Spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
780
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
781
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 50 μm |