2 micrographs for composition Fe, C 3.6, Si 2.1 (wt%), ordered by micrograph number.
![]() |
Micrograph
62
:
Fe, C 3.6, Si 2.1 (wt%), hypereutectic grey cast iron System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
63
:
Fe, C 3.6, Si 2.1 (wt%), hypereutectic grey cast iron System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1 (wt%) Reflected light microscopy 40 μm |