Composition
1 micrograph for composition Stainless steel with Nb 1 (wt%), ordered by micrograph number.
![]() |
Micrograph
800
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Nb 1 (wt%) Scanning electron microscopy (SEM) 1 μm |