Composition
2 micrographs for composition Fe, C 0.12, Mn 14.2, Cr 13.7, ordered by micrograph number.
![]() |
Micrograph
806
:
Austenitic stainless steel water quenched then cooled, showing transformation to g in the a lamellae System: Fe-C-X, Composition: Fe, C 0.12, Mn 14.2, Cr 13.7 Reflected light microscopy 50 μm |
![]() |
Micrograph
831
:
Austenitic stainless steel water quenched, with a-martensite needles within lamellae System: Fe-C-X, Composition: Fe, C 0.12, Mn 14.2, Cr 13.7 Scanning electron microscopy (SEM) 4 μm |