Composition
1 micrograph for composition Al, Mg 1, Si 0.8, Mn 0.5 (wt%), ordered by micrograph number.
![]() |
Micrograph
843
:
Micrograph of base metal. T6 - solution heat treated and artificially aged. System: Al-Mg-Si, Composition: Al, Mg 1, Si 0.8, Mn 0.5 (wt%) Optical microscope, reflected light 250 μm |