Composition
2 micrographs for composition Notched zinc, ordered by micrograph number.
![]() |
Micrograph
75
:
Notched zinc, broken by impact at room temperature System: Zn, Composition: Notched zinc Scanning electron microscopy (SEM) 1 mm |
![]() |
Micrograph
76
:
Notched zinc, broken by impact at room temperature System: Zn, Composition: Notched zinc Scanning electron microscopy (SEM) 160 μm |