1 micrograph for composition Not specified (System: Hydroxyapatite (Ca10(PO4)6(OH)2)), ordered by micrograph number.
![]() |
Micrograph
117
:
Sintered disc of Hydroxyapatite (Ca10(PO4)6(OH)2), a calcium phosphate ceramic with similar composition to natural bone mineral System: Hydroxyapatite (Ca10(PO4)6(OH)2), Composition: Not specified Scanning electron microscopy (SEM) 18 μm |