Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Composition
2 micrographs for composition Bi 60, Cd 40 (wt%), ordered by micrograph number.
![]() |
Micrograph
6
:
Bi 60, Cd 40 (wt%), eutectic alloy System: Bi-Cd, Composition: Bi 60, Cd 40 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
7
:
Bi 60, Cd 40 (wt%), eutectic alloy System: Bi-Cd, Composition: Bi 60, Cd 40 (wt%) Reflected light microscopy 40 μm |