Composition
1 micrograph for composition Al2O3, C up to 30 (wt%), Si few%, ordered by micrograph number.
![]() |
Micrograph
151
:
Alumina-graphite brick System: Al2O3-C-Si, Composition: Al2O3, C up to 30 (wt%), Si few% Reflected light microscopy 400 μm |