6 micrographs for composition Not specified (System: LAS: Li2O-Al2O3-SiO2), ordered by micrograph number.
![]() |
Micrograph
160
:
Glass ceramic, heat treated at 750° C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
161
:
Glass ceramic, heat treated at 750°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy 100 μm |
![]() |
Micrograph
162
:
Glass ceramic, heat treated at 840°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
163
:
Glass ceramic, heat treated at 840°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy 100 μm |
![]() |
Micrograph
164
:
Glass ceramic, heat treated at 900°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
165
:
Glass ceramic, heat treated at 900°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy 100 μm |