Composition
2 micrographs for composition Cu 70, Ni 30 (wt%), ordered by micrograph number.
![]() |
Micrograph
10
:
Cu 70, Ni 30 (wt%), cored dendrites System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
11
:
Cu 70, Ni 30 (wt%), cored dendrites System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%) Reflected light microscopy 80 μm |