Composition
1 micrograph for composition ZrO2 5-30, Al2O3 70-95 (wt%), ordered by micrograph number.
![]() |
Micrograph
195
:
Zirconia Toughened Alumina (ZTA) System: ZrO2-Al2O3, Composition: ZrO2 5-30, Al2O3 70-95 (wt%) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |