Composition
1 micrograph for composition BaTiO3 95-97 (wt%), ordered by micrograph number.
![]() |
Micrograph
199
:
BaTiO3 Temperature-stable dielectric capacitor System: BaTiO3 + other oxides such as Nb2O5, Bi2O3, Composition: BaTiO3 95-97 (wt%) Bright-field TEM 1 μm |