2 micrographs for composition Fe, C 0.55 (wt%), ordered by micrograph number.
![]() |
Micrograph
225
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.55 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
226
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.55 (wt%) Reflected light microscopy 200 μm |