Composition
3 micrographs for composition Fe, C 0.5 (wt%), ordered by micrograph number.
![]() |
Micrograph
229
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
230
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.5 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
268
:
Fe, C 0.5 (wt%) steel, near a decarburised surface System: Fe-C-X, Composition: Fe, C 0.5 (wt%) Reflected light microscopy 400 μm |