4 micrographs for composition Fe, C 0.6 (wt%), ordered by micrograph number.
![]() |
Micrograph
231
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.6 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
232
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.6 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
269
:
Fe, C 0.6 (wt%) steel, hard drawn System: Fe-C-X, Composition: Fe, C 0.6 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
270
:
Fe, C 0.6 (wt%) steel, hard drawn System: Fe-C-X, Composition: Fe, C 0.6 (wt%) Reflected light microscopy 200 μm |