Composition
8 micrographs for composition Fe, C 1.3 (wt%), ordered by micrograph number.
![]() |
Micrograph
243
:
Fe, C 1.3 (wt%) steel, annealed at 1100°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
244
:
Fe, C 1.3 (wt%) steel, annealed at 1100°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
245
:
Fe, C 1.3 (wt%) steel, normalised at 1050°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
246
:
Fe, C 1.3 (wt%) steel, normalised at 1050°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
247
:
Fe, C 1.3 (wt%) steel, normalised at 1050°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
248
:
Fe, C 1.3 (wt%) steel, annealed at 1000°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
249
:
Fe, C 1.3 (wt%) steel, annealed at 1000°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
250
:
Fe, C 1.3 (wt%) steel, annealed at 1000°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 100 μm |