3 micrographs for composition Fe, C 0.55, Mn 0.65 (wt%), ordered by micrograph number.
![]() |
Micrograph
278
:
Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
279
:
Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite and cracking System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
280
:
Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite and cracking System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%) Reflected light microscopy 100 μm |