Composition
8 micrographs for composition Fe, C 0.4 (wt%), ordered by micrograph number.
![]() |
Micrograph
290
:
Fe, C 0.4 (wt%) steel, quenched, martensitic and quench cracks System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
291
:
Fe, C 0.4 (wt%) steel, quenched, martensitic and quench cracks System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
292
:
Fe, C 0.4 (wt%) steel, quenched, martensitic and quench cracks System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
293
:
Fe, C 0.4 (wt%) steel, quenched, martensitic System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
309
:
Fe, C 0.4 (wt%) steel, slow quenched System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
310
:
Fe, C 0.4 (wt%) steel, slow quenched System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
311
:
Fe, C 0.4 (wt%) steel, slow quenched System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
312
:
Fe, C 0.4 (wt%) steel, slow quenched System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |