Contributor
320 micrographs contributed by Dr R F Cochrane, ordered by micrograph number.
Showing 151 - 160 of 320 micrographs | Page 1 .. 13 14 15 16 17 18 19 .. 32 | Previous | Next |
Micrograph
361
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
362
:
White cast iron, subject to slow heating and cooling treatment System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
363
:
White cast iron, subject to slow heating and cooling treatment System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
364
:
White cast iron, subject to slow heating and cooling treatment System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
365
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), + ... Reflected light microscopy 200 μm |
|
Micrograph
366
:
Whiteheart cast iron System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), + ... Reflected light microscopy 400 μm |
|
Micrograph
367
:
Whiteheart cast iron System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), + ... Reflected light microscopy 200 μm |
|
Micrograph
368
:
Blackheart cast iron System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
369
:
Blackheart cast iron System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
370
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.85, Si 0.33, Mn 0.39, Cr 0.91 (wt%) Reflected light microscopy 400 μm |
Showing 151 - 160 of 320 micrographs | Page 1 .. 13 14 15 16 17 18 19 .. 32 | Previous | Next |