Contributor
320 micrographs contributed by Dr R F Cochrane, ordered by micrograph number.
Showing 161 - 170 of 320 micrographs | Page 1 .. 14 15 16 17 18 19 20 .. 32 | Previous | Next |
Micrograph
371
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.85, Si 0.33, Mn 0.39, Cr 0.91 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
372
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 3.62, Si 0.33, Mn 0.38, Cr 0.89 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
373
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 3.62, Si 0.33, Mn 0.38, Cr 0.89 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
374
:
Fully transformed ledeburite cast iron System: Fe-C-X, Composition: Fe, C 4.17, Si 0.40, Mn 0.45, Cr 0.95 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
375
:
Fully transformed ledeburite cast iron System: Fe-C-X, Composition: Fe, C 4.17, Si 0.40, Mn 0.45, Cr 0.95 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
376
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 3.56, Si 0.20, Mn 0.37, Cr 0.91 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
377
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 3.56, Si 0.20, Mn 0.37, Cr 0.91 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
378
:
Grey cast iron with significant Si content System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron) Reflected light microscopy 400 μm |
|
Micrograph
379
:
Grey cast iron with significant Si content System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron) Reflected light microscopy 200 μm |
|
Micrograph
380
:
Grey cast iron with significant Si content System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron) Reflected light microscopy 100 μm |
Showing 161 - 170 of 320 micrographs | Page 1 .. 14 15 16 17 18 19 20 .. 32 | Previous | Next |