Contributor
320 micrographs contributed by Dr R F Cochrane, ordered by micrograph number.
Showing 171 - 180 of 320 micrographs | Page 1 .. 15 16 17 18 19 20 21 .. 32 | Previous | Next |
Micrograph
381
:
Grey cast iron System: Fe-C-X, Composition: Grey cast iron Reflected light microscopy 400 μm |
|
Micrograph
382
:
Grey cast iron System: Fe-C-X, Composition: Grey cast iron Reflected light microscopy 200 μm |
|
Micrograph
383
:
Grey cast iron System: Fe-C-X, Composition: Grey cast iron Reflected light microscopy 100 μm |
|
Micrograph
384
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
385
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
386
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
387
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 400 μm |
|
Micrograph
388
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 200 μm |
|
Micrograph
389
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 100 μm |
|
Micrograph
390
:
Nickel hard cast iron, martensitic System: Fe-C-X, Composition: Fe, C 2.95, Si 0.60, Mn 0.60, Ni 4.00, Cr 1.90 (wt%) Reflected light microscopy 400 μm |
Showing 171 - 180 of 320 micrographs | Page 1 .. 15 16 17 18 19 20 21 .. 32 | Previous | Next |