Contributor
320 micrographs contributed by Dr R F Cochrane, ordered by micrograph number.
Showing 221 - 230 of 320 micrographs | Page 1 .. 20 21 22 23 24 25 26 .. 32 | Previous | Next |
Micrograph
431
:
Cu 80, Zn 20 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
432
:
Cu 80, Zn 20 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
433
:
Cu 90, Zn 10 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 90, Zn 10 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
434
:
Cu 90, Zn 10 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 90, Zn 10 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
435
:
Tough pitch' nearly pure copper, with oxygen impurity System: Cu, Composition: Cu 99.7 (wt%), some oxygen Reflected light microscopy 400 μm |
|
Micrograph
436
:
Tough pitch' nearly pure copper, with oxygen impurity System: Cu, Composition: Cu 99.7 (wt%), some oxygen Reflected light microscopy 200 μm |
|
Micrograph
437
:
Cu, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
438
:
Cu, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
439
:
a b nickel brass containing 2% lead. System: Cu-Zn, Composition: Cu 46, Zn 42, Ni 10, Pb 2 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
440
:
a b nickel brass containing 2% lead. System: Cu-Zn, Composition: Cu 46, Zn 42, Ni 10, Pb 2 (wt%) Reflected light microscopy 400 μm |
Showing 221 - 230 of 320 micrographs | Page 1 .. 20 21 22 23 24 25 26 .. 32 | Previous | Next |