Contributor
320 micrographs contributed by Dr R F Cochrane, ordered by micrograph number.
Showing 301 - 310 of 320 micrographs | Page 1 .. 26 27 28 29 30 31 32 | Previous | Next |
Micrograph
518
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 200 μm |
|
Micrograph
519
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 100 μm |
|
Micrograph
520
:
Cu - 5% Sn phosphor bronze. System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx) Reflected light microscopy 400 μm |
|
Micrograph
521
:
Cu - 5% Sn phosphor bronze. System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx) Reflected light microscopy 200 μm |
|
Micrograph
522
:
Cu - 5% Sn phosphor bronze. System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx) Reflected light microscopy 100 μm |
|
Micrograph
523
:
Phosphor bronze exhibiting cored dendrites. System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) + P trace Reflected light microscopy 400 μm |
|
Micrograph
524
:
Phosphor bronze exhibiting cored dendrites. System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) + P trace Reflected light microscopy 200 μm |
|
Micrograph
525
:
Phosphor bronze exhibiting cored dendrites. System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) + P trace Reflected light microscopy 100 μm |
|
Micrograph
526
:
Cast and tempered 20% Sn bronze System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
527
:
Cast and tempered 20% Sn bronze System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 400 μm |
Showing 301 - 310 of 320 micrographs | Page 1 .. 26 27 28 29 30 31 32 | Previous | Next |