Contributor
320 micrographs contributed by Dr R F Cochrane, ordered by micrograph number.
Showing 51 - 60 of 320 micrographs | Page 1 .. 3 4 5 6 7 8 9 .. 32 | Previous | Next |
Micrograph
251
:
Fe, C 0.8 (wt%) steel, eutectoid transformation, normalised at 900ºC System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
252
:
Fe, C 0.8 (wt%) steel, eutectoid transformation, normalised at 900ºC System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
253
:
Fe, C 1 (wt%) steel, normalised hypereutectoid System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
254
:
Fe, C 1 (wt%) steel, normalised hypereutectoid System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
255
:
Fe, C 1.1 (wt%) steel, normalised hypereutectoid System: Fe-C-X, Composition: Fe, C 1.1 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
256
:
Fe, C 1.1 (wt%) steel, normalised hypereutectoid System: Fe-C-X, Composition: Fe, C 1.1 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
260
:
Eutectoid steel, normalised System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
261
:
Eutectoid steel, normalised System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
262
:
Eutectoid steel, normalised System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
263
:
Eutectoid steel, normalised System: Fe-C-X, Composition: Fe, C 0.8 (wt%) Reflected light microscopy 200 μm |
Showing 51 - 60 of 320 micrographs | Page 1 .. 3 4 5 6 7 8 9 .. 32 | Previous | Next |