DoITPoMS

Contributor

44 micrographs contributed by Dr K M Knowles, ordered by micrograph number.


Showing 1 - 10 of 44 micrographs Page 1 2 3 4 5 | Previous | Next

Link to full record for micrograph 160 Micrograph 160 : Glass ceramic, heat treated at 750° C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 161 Micrograph 161 : Glass ceramic, heat treated at 750°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy
100 μm
Link to full record for micrograph 162 Micrograph 162 : Glass ceramic, heat treated at 840°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 163 Micrograph 163 : Glass ceramic, heat treated at 840°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy
100 μm
Link to full record for micrograph 164 Micrograph 164 : Glass ceramic, heat treated at 900°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy, with sensitive tint plate
100 μm
Link to full record for micrograph 165 Micrograph 165 : Glass ceramic, heat treated at 900°C for 3 hours
System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified
Transmitted polarised light microscopy
100 μm
Link to full record for micrograph 166 Micrograph 166 : Carbon-carbon composite
System: CCcomposite, Composition: Not specified
Reflected light microscopy
250 μm
Link to full record for micrograph 167 Micrograph 167 : Carbon-carbon composite
System: CCcomposite, Composition: Not specified
Reflected light microscopy
100 μm
Link to full record for micrograph 168 Micrograph 168 : Carbon-carbon composite
System: CCcomposite, Composition: Not specified
Reflected light microscopy
250 μm
Link to full record for micrograph 169 Micrograph 169 : Carbon-carbon composite
System: CCcomposite, Composition: Not specified
Reflected light microscopy
40 μm

Showing 1 - 10 of 44 micrographs Page 1 2 3 4 5 | Previous | Next

List all contributors