Contributor
2 micrographs contributed by Dr P J Barham, ordered by micrograph number.
![]() |
Micrograph
555
:
Banded spherulites in a blend of polyethtylenes System: Polyethylene (PE), Composition: LPE:BPE 1:3 Transmission electron microscopy (TEM) 200 nm |
![]() |
Micrograph
556
:
Sheaf-like arrangement of lamellae in a blend of polyethylenes System: Polyethylene (PE), Composition: LPE:BPE 3:1 Transmission electron microscopy (TEM) 200 nm |