Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Contributor
104 micrographs contributed by Dr Ingo Keesmann, ordered by micrograph number.
| Showing 1 - 10 of 104 micrographs | Page 1 2 3 4 5 6 7 .. 11 | Previous | Next |
![]() |
Micrograph
872
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production. System: Cu production, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
873
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production. System: Cu production, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
874
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production. System: Cu production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
875
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production.. System: Cu production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
876
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production. System: Cu production, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
877
:
Los Millares, Almeria, Spain. Chalcolithic (arsenical)-copper production. System: Cu production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
878
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Smithing slag, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
879
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag System: Smithing slag, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
880
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Smithing slag, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
881
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Smithing slag, Composition: Not specified Reflected light microscopy 200 μm |