104 micrographs contributed by Dr Ingo Keesmann, ordered by micrograph number.
| Showing 101 - 104 of 104 micrographs | Page 1 .. 5 6 7 8 9 10 11 | Previous | Next |
![]() |
Micrograph
972
:
Smithing slag Carthage, phoenician System: Smithing slag, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
973
:
Dasht-e-Kavir, Saghand, Central Iran. Lead slag System: Pb, Composition: Not specified Transmitted light microscopy 500 μm |
![]() |
Micrograph
974
:
Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag System: Cu production, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
975
:
Dasht-e-Kavir, Saghand - Posht-e-Badam. Copper slag System: Cu production, Composition: Not specified Transmitted light microscopy 200 μm |