Contributor
104 micrographs contributed by Dr Ingo Keesmann, ordered by micrograph number.
| Showing 11 - 20 of 104 micrographs | Page 1 2 3 4 5 6 7 .. 11 | Previous | Next |
![]() |
Micrograph
882
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Smithing slag, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
883
:
Hambach forest, Germany. Medieval smithing slag System: Smithing slag, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
884
:
Monte Romero, Huelva district, Spain. Phoenician, preroman silverproduction from complex ores. System: Pre-Roman Ag production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
885
:
Monte Romero, Huelva district, Spain. Phoenician, preroman silver production from complex ores. System: Pre-Roman Ag production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
886
:
Maroni, Cyprus, copper slag System: Cu production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
887
:
Maroni, Cyprus, copper slag System: Cu production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
888
:
Maroni, Cyprus, copper slag System: Cu production, Composition: Not specified Reflected light microscopy 1 mm |
![]() |
Micrograph
889
:
Timna, wadi Arabah, Negev, Israel System: Cu production, Composition: Not specified Transmitted light microscopy 500 μm |
![]() |
Micrograph
890
:
Monte Romero, Huelva district, Spain. Phoenician, preroman silver production from complex ores. System: Pre-Roman Ag production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
891
:
Monte Romero, Huelva district, Spain. Phoenician, preroman silver production from complex ores. System: Pre-Roman Ag production, Composition: Not specified Reflected light microscopy 500 μm |