Contributor
104 micrographs contributed by Dr Ingo Keesmann, ordered by micrograph number.
| Showing 81 - 90 of 104 micrographs | Page 1 .. 5 6 7 8 9 10 11 | Previous | Next |
![]() |
Micrograph
952
:
Afunfun, Niger. Melilith-pyroxene-copper slag System: Cu production, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
953
:
Afunfun, Niger. Melilith-pyroxene-slag System: Cu production, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
954
:
Afunfun, Niger. Melilith-pyroxene-copper slag System: Cu production, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
955
:
Afunfun, Niger. Melilith-pyroxene-copper slag System: Cu production, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
956
:
Carthage, smithing slag, phoenician System: Smithing slag, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
957
:
Kupferberg, Fichtel mountain, Germany. Speiss from copper production System: Cu production, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
958
:
Kupferberg, Fichtel mountain, Germany. Speiss from copper production System: Cu production, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
959
:
Carthage, smithing slag, phoenician System: Smithing slag, Composition: Not specified Transmitted light microscopy 1 mm |
![]() |
Micrograph
960
:
Fichtel mountain, Germany. Subrecent iron slag System: Fe production, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
961
:
Torud, Central Iran. Copper slag System: Cu production, Composition: Not specified Reflected light microscopy 500 μm |