Micrograph no
30
Brief description
Cu 70, Zn 30 (wt%), annealed and cold rolled
Keywords
alloy Link to MATTER Glossary entry for alloy, annealing Link to MATTER Glossary entry for annealing, brass Link to MATTER Glossary entry for brass, copper, dislocation Link to MATTER Glossary entry for dislocation, metal, slip band Link to MATTER Glossary entry for slip band, zinc
Categories
Metal or alloy
System
Cu-Zn   Link to phase diagram
Composition
Cu 70, Zn 30 (wt%)
Standard codes
Reaction
Processing
Annealed and cold rolled 50%
Applications
Sample preparation
Technique
Reflected light microscopy
Length bar
40 μm
Further information
This sample was annealed and 50% cold rolled to give a highly deformed structure with a high dislocation density, illustrated by the large number of persistent slip bands.
Contributor
Prof T W Clyne
Organisation
Department of Materials Science and Metallurgy, University of Cambridge
Date
25/10/01
Licence for re-use
Attribution-Non-Commercial-Share Alike 2.0 UK: England & Wales
Related micrographs