DoITPoMS

Full Record for Micrograph 420

Link to full size image of micrograph 420
[280 KB]

View micrograph
.. in new window

View micrograph and record
.. in new window


You can also view and download the micrographs at CORE-Materials and also on Flickr
Micrograph no
420
Brief description
Commercial brass, ~30% Zn, displaying dendritic solidification
Keywords
Query failed with error :