Full Record for Micrograph 691
[143 KB]
View micrograph
.. in new window
View micrograph and record
.. in new window
You can also view and download the micrographs on Flickr
- Micrograph no
- 691
- Brief description
- Silicon carbide
- Keywords
- ceramic
, silicon carbide - Categories
- Ceramic
- System
- SiC
- Composition
- Not specified
- Standard codes
- Reaction
- Processing
- Applications
- Sample preparation
- Etched in K<sub>3</sub>Fe(CN)<sub>6</sub> + NaOH + H<sub>2</sub>O (boiled to dryness).
- Technique
- Reflected light microscopy
- Length bar
- 100 μm
- Further information
- Contributor
- Dr J Marrow
- Organisation
- Department of Materials Science, University of Manchester and UMIST
- Date
- 07/11/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs