Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Full Record for Micrograph 8
[120 KB]
View micrograph
.. in new window
View micrograph and record
.. in new window
You can also view and download the micrographs on Flickr
- Micrograph no
- 8
- Brief description
- Bi 80, Cd 20 (wt%), hypereutectic alloy
- Keywords
- alloy
, bismuth, cadmium, dendrite
, facet
, hypereutectic
, metal - Categories
- Metal or alloy
- System
- Bi-Cd
- Composition
- Bi 80, Cd 20 (wt%)
- Standard codes
- Reaction
- Processing
- Slowly cooled from liquid
- Applications
- Sample preparation
- Etched in alcoholic FeCl3
- Technique
- Reflected light microscopy
- Length bar
- 400 μm
- Further information
- The high proportion of Bi in this sample results in predominantly Bi dendrites with some interdendritic eutectic. The primary Bi dendrites are strongly facetted (white blocks) indicating the importance of crystallographic orientation upon growth.
- Contributor
- Prof T W Clyne
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 25/10/01
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs